About Leather Tanning
Tanning begins by soaking hides and scraping away hair and fat, then treating them with local plant tannins such as pomegranate rind and tree bark until they soften and resist decay. Once dry, the hides are stretched and polished, ready to be shaped.
Tanning served nomadic and settled life alike: leather was the material of water skins, buckets, saddles and bags.
How it is made
-
Step 1: Soaking and cleaning the hides
-
Step 2: Removing hair and fat
-
Step 3: Steeping in tanning agents
-
Step 4: Drying and stretching
-
Step 5: Polishing and softening
Tools
- Scraper
- Soaking vats
- Knife
Raw materials
- Goat and camel hides
- Pomegranate rind
- Tree bark
- Salt
- Water